Flite Technology’s 38 Step General Procedure For Feed Screw Rebuilding
Primary Flights Only

  1. Prepare screw for pre-work inspection. Remove plastic, rust, etc., utilizing chemical cleaners, heat of grit blasters, as required.
  2. Complete detailed pre-work inspection report. Record  screw LD. Numbers, flight O.D.s, flight O.D.s, flight widths widths, root O.D.s, O.A.L. seal dimensions, drive conditions, Rockwell hardness, itemizes additional damage, and  a wear analysis is implemented.
  3. Screws are checked for metal fatigue, cracks by dye penetrant or megna flux testing. (Note: As through as feed screws are inspected, some cracks do not show up until they are being welded or ground. Hence, screws are checked a number of times during the rebuilding process.)
  4. Processors is called to confirm price, delivery and scope of repair before any work is done.
  5. Customers requesting blueprints of their screws for future placement of manufacture orders are made at this time.
  6. Detailed four page, step-by-step work orders are issued to the shop. Work orders have questions for each machine operator to state the method, material, and dimension or specifications obtained at his work station.
  7. Screws are centered and straightened, removable tips are taken off, and tip counterbores are checked for concentricity.
  8. Hard chrome or other plantings/coatings, if present on the root diameter, are chemically removed.
  9. Stress relieving is done as required.
  10. Existing hardfacing is entirely ground off. Some of our competitors try welding new hardfacing onto old hardfacing to save money and then wonder why it is full of cracks and falling off.
  11. If screws are extremely undersized or have to be severely underground to remove existing hardfacing, a “buffer” layer of steel may be applied between the new hardfacing and the base metal of the screws.
  12. Screws are pre-heated and maintained to exact temperatures required for specific hardfacing material and welding methods.
  13. Major weld repairs of modifications are completed. Serious flight width deterioration is rectified. Please note:  Flite Technology, Inc., considers minors root repairs, bearing section and register rebuilding as part of the rebuilding process and does not charge for this additional work or service.
  14. Flight surfaces are cleaned with chemical solvents and/or abrasive which  is required for excellent adherence.
  15. Hardfacing is applied. Welded samples, is required, are available for metallurgical and microstructure evaluation.
  16. Screws are immediately placed in and covered with a vermiculite for nad approximate 48 hours cool down period to eliminate cracking as much as possible.
  17. Stress relieving is done, as required.
  18. Straightened occurs.
  19. Rough grind screws to an even over-size dimension.


 


North American Feed Screw and Barrel Manufacturers-Rebuilders Assoc.
Corporate 2511 N Friday Rd.
Cocoa, Florida 32926
United States
321-631-2050, 800-327-9310
FAX - 321-636-3508
flitetech@gmail.com
Para Spanish Teléfono: 321-433-3315

419 Hawk St Rockledge FL.32955
440 Shearer Blvd Cocoa Fl. 32922
Atlanta GA 30342
North Royalton OH 44133
Lynchburg, VA 24502
Brodheadsville, PA 18322
Andover, MA 01810
Detroit MI 48393
Ontario Canada
Playas de Coco Costa Rica
Plus 15 other affiliated facilities throughout USA & Canada

WORLD SOURCING - DISTRIBUTION